Internet resources for ceramics are growing every day. You can participate in
discussions with thousands of people many of whom have years of experience. Check our links page for a springboard into the ceramic internet.
- INSIGHT for Windows or Macintosh is an ceramic
calculator and empowers you to take control of your glazes with confidence and power you
never dreamed possible. It is totally focussed on doing classic
ceramic calculations at lightning speed and you can do two at once
to compare them side-by-side. It is ideal for education (i.e. demonstrating
the concepts of unity, analysis, formula,
and LOI are easy).
- FORESIGHT is a DOS stand-alone relational ceramic
database system that maintains unlimited materials, oxides,
recipes, test procedures, test results,
physical property, reference, and people data in the industry-standard Foxpro file and
index format. It has a calculation engine that automatically generates analysis, formula,
and cost data for materials and recipes.
- Our Magic of Fire book will prepare you for
the world of ceramic calculations and database systems and it will introduce you
to simple yet effective physical testing you can do now. It is closely integrated with our
software and helps readers intelligently decide when ceramic calculations are appropriate
and when they should give way to physical testing.
Ancient potters prayed to the kiln god to watch over their firings, today they would
likely take advantage of available technology.
- The 'need-know-only' culture in industry needs a funeral. You need in-house expertise,
don't rely on suppliers or consultants only.
- That storage room full of mysterious materials bought just to test
failed recipes is a monument to a passive mindset that needs to
die among potters.
- Understand glazes and materials, don't just use them. What is in each
material and why it is there? The implications of removing or altering each ingredient?
Changing the firing? Using with oxides and opacifiers?
- Stop spinning your wheels. Stop having failures and learning nothing
from them.
- Develop opinions.
Abandon Obsolete Thinking
In past we had glaze books filled with cantankerous recipes. Now it is better to have
only a few base glazes and adjust these to produce all the needed effects. You should be
able to draw a 'family tree' of all your recipes showing how they interrelate and the
rationalization for specific alterations.
- It is impossible to control 50 recipes. It is much better to start
with one base glossy and one base matte, preferably closely related. This
approach allows you to concentrate your efforts on understanding and perfecting the
properties of one base. Improvements to the base will benefit every glaze derived from it.
You'll be able to throw out all those bags of materials you bought just to test recipes
that never worked
- A recipe and the documentation that rationalizes it are inseparable entities
where beginners are the recipients. Unfortunately the very ones who trade most are those
who have not reached the 'want-to-know-why' stage. There are 'ethics'
giver and receiver should not ignore. Documented recipes prove the author is conscientious
and willing to field questions to help users adapt. Recipients willing to 'understand' and
adjust demonstrate a grasp of the true nature of ceramic processes. Poor glazes can injure
people physically.
- Reliance on 'Textbook recipes'
is a constant impediment to your progress. They will control you instead of you them,
they'll throw good results almost totally to chance, they are an impediment to your
progress. They will stand as a barrier between you and getting an understanding, being in
touch. Like raising and training a puppy from birth, it will just be easier to create your
own recipes.
Keeping Good Records
- Did you do a lot of testing in the past 15 years? Where are the results? It is a shame
not to learn from your own past. FORESIGHT completely
replaces your existing record keeping system. With it you can store a life time of ceramic
related information in an organized, searchable, reportable format. Every piece of paper
on your desk, in your filing cabinets could be in FORESIGHT where you can find it.
- Instead of searching filing cabinets and boxes, you should be searching your database.
- Your plant should have documentation on each material used, there should be notes that
clearly rationalize advantages and disadvantages compared to alternative products and
factors about the material that require extra diligence in production and testing to
assure quality.
Determination for Technical Excellence
- In the past our consciences allowed us to put 90% of our effort on appearance and 10% on
technical issues. Accept your responsibility to produce ware that is beautiful but also
hard, strong, dense, acid resistant, thermal shock resistant, chip resistant, and pinhole
and craze free.
- Don't be intimidated by the simple techniques and tools that are within your reach now.
You might consider Prayer if our solutions do not work!