We are working on this database and would appreciate if you can help us add materials and improve the alternate name in this list. Our objective is to include generic materials in each MDT and maintain name-brand versions of these for each area of the world. In education, the generic or theoretical materials are employed in ceramic calculations, whereas in industry the chemistries for the specific materials are used.

The MDT download page offers the ability to maintain a custom MDT file (you have to be logged in to do this). On the download page you can choose this MDT as the starter and then add any material (from the thousands available). You can also change the name of any of the materials you add thus you can translate the table into your language. You can add any material (even ones that are already in this starter MDT) for the purpose of changing the name. Then generate the MDT and download it (and put it in the INSIGHT data folder).

In Bound Links

  • (Materials) BPS Cornish Stone
  • (Materials) BPS Low Expansion Frit - High calcium boro aluminum silicate frit
  • (Materials) BPS Feldspar
  • (Materials) Bone Ash Calcined - Ca3(PO4)2
  • (Materials - Member) Super Standard Porcelain - White burning high strength Cornish kaolin

    Super Standard Porcelain Kaolin

  • (Materials - Member) Frit P2955 - High alkali low alumina borax frit

    PotteryCrafts Frit 2955

  • (Materials) BPS Soda Feldspar
  • (Materials) BPS Lead Bisilicate - Lead alumina bilsilicate frit
  • (Materials) BPS High Alkaline Frit - Frit
  • (Materials - Member) Standard Porcelain Kaolin - A white burning high strength Cornish kaolin

    English Standard Porcelain, Eng Stn Porc, Standard Porcelain China Clay

  • (Materials - Member) Hyplas 71 Ball Clay - Devon medium strength low iron ball clay
  • (Materials - Member) Treviscoe Kaolin - A white burning high strength Cornish kaolin

    Treviscoe China Clay

  • (Materials - Member) Hymod AT Ball Clay - Dorset brown burning high strength ball clay
  • (Materials - Member) Calcined Alumina - Al2O3 - Aluminum oxide

    Alumina Calcined, Calcnd Alum, Ground Alumina, Corundum

  • (Materials - Member) Alumina Hydrate - Al2O3.3H2O

    Alum Hydrate, Alumina Trihydrate, Hydrated Alumina, Alpha Aluminum Trihydroxide, Gibbsite

  • (Materials - Member) Anhydrous Borax - Na2B4O7 - Fused Borax, Sodium Tetraborate

    Calcined Borax, Dehydrated Borax, Pyrobor

  • (Materials - Member) Ball Clay - Highly Plastic Fine Particle Clay
  • (Materials - Member) Barium Carbonate - BaCO3

    Barium Carb, Witherite

  • (Materials - Member) Bentonite

    Montmorillonite

  • (Materials - Member) Bone Ash - Ca5(OH)(PO4)3

    Calcium Phosphate

  • (Materials - Member) Borax Pentahydrate - Na2B4O7.5H2O - Etibor-48

    Borax 5 Mol, Sodium Tetraborate, Borax 5-hydrate

  • (Materials - Member) Boric Acid - H3BO3 or B2O3.3H2O

    Boracic acid, Orthoboric Acid, Hydrous Boric Oxide

  • (Materials - Member) Calcined Kaolin - Al2O3.2SiO2

    Cal Kaolin

  • (Materials - Member) Calcium Carbonate - CaCO3

    Carbonate of Lime, Whiting, Aragonite, Calcite, CaCO3

  • (Materials - Member) Calcium Feldspar - CaO.Al2O3.4SiO2 or CaAl2Si2O8

    Lime Spar, Lime Feldspar, Ca-Feldspar

  • (Materials - Member) Colemanite - 2CaO.3B2O3.5H2O or CaB3O4(OH)3·H2O
  • (Materials - Member) Cornwall Stone

    Cornish Stone, China Stone, Corn Stn, China-stone

  • (Materials - Member) Cryolite - Na3AlF6

    Cryloite, Sodium Fluoaluminate, Kryolith

  • (Materials - Member) Dolomite - CaCO3.MgCO3 or CaMg(CO3)2 - Double carbonate of magnesia/calcia

    Calcium Magnesium Carbonate, Raw Limestone

  • (Materials - Member) Magnesite - MgCO3

    Mag Carb, MgCO3, Anhydrous Magnesium Carbonate

  • (Materials - Member) Borax Decahydrate - Na2B4O7.10H2O

    Sodium TetraBorate Decahydrate, Borax 10-hydrate, 10 Mol Borax, Neobor

  • (Materials - Member) Sodium Carbonate Heptahydrate - Na2CO3.7H2O - A source of sodium in the glass industry
  • (Materials) Ceramic Rutile - TiO2

    Calcined Rutile, Light Rutile, Rutile Ceramic

  • (Materials) BPS Calcium Borate Frit - Calcium Borate Frit
  • (Materials - Member) Ilmenite - FeTiO3 or FeO.TiO2 - Iron & Titanium Oxide

    Illmenite, Ferrous Titanate, Iron Titanate

  • (Materials - Member) Iron Oxide Yellow - FeO.OH or Fe2O3.H2O - Fe2O3.H2O, FeO(OH), Goethite

    Iron(III) oxide, hydrated iron oxide, iron(III) hydroxide

  • (Materials - Member) Lead Monosilicate Frit
  • (Materials - Member) Frit P2953 - Borax frit

    PotteryCrafts Frit 2953

  • (Materials - Member) Frit P2954 - Calcium Borate Frit similar to Gerstley Borate

    PotteryCrafts Frit 2954

  • (Materials - Member) Frit P2957 - Low expansion borax frit

    PotteryCrafts Frit P2957

  • (Materials - Member) Frit P2961 - Standard alkaline frit

    PotteryCrafts Frit P2961

  • (Materials - Member) Frit P2960 - Low Expansion Frit

    PotteryCrafts Frit 2960

  • (Materials - Member) Frit P3110 - This is actually Ferro Frit 3110

    PotteryCrafts Frit P3110

  • (Materials - Member) Frit P2962 - High alkaline frit

    PotteryCrafts Frit P2962

  • (Materials - Member) Potclays Frit 2261 - Lead alumina bilsilicate frit

    Potclays Lead Bisilicate Frit

  • (Materials - Member) Potclays Frit 2263 - High calcium borosilicate frit

    2263 Standard boraksfritte, Potclays Standard Borax Frit

  • (Materials - Member) Potclays Frit 2279 - Alkali free calcium lithium magnesia zinc borosilicate frit

    2279 Fritte, Potclays Low Expansion Frit

  • (Materials - Member) Potclays Frit 2275 - Very high alkali frit

    2275 Alkalifritte, Potclays High Alkali Frit

  • (Materials - Member) Potclays Frit 2262 - Lead Frit

    2262 Bly halvannensilicat, Potclays Lead Sesquisilicate Frit

  • (Materials - Member) Potclays Frit 2270 - White Zircon Frit

    2270 Hvit zircon Boraks fritte, Potclays White Zircon Borax Frit

  • (Materials - Member) Potclays Frit 2268 - Very high calcium borosilicate frit

    2268 Kasiumborat fritte, Potclays Calcium Borate Frit

  • (Materials - Member) Potclays Frit 2265

    Potclays H.T. Borax Frit

  • (Materials - Member) Potclays Frit 2266 - This is actually Ferro Frit 3110

    Potclays Ferro Crystal Frit

  • (Materials - Member) English Kaolin - Al2O3.SiO2 - White Burning High Flux Kaolin
  • (Materials - Member) Calcium Borate - Ca(BO2)2 or CaO.B2O3

    Anhydrous Borocalcite

  • (Materials - Member) Fluorspar - CaF2

    Fluorite, Calcium Fluoride, Blue John

  • (Materials - Member) Iron Oxide Red - Fe2O3 - Synthetic Hematite

    Ferric Oxide, Red Iron Oxide, RIO, Iron(III) oxide, Fe2O3, Hematite

  • (Materials - Member) Kaolin - Al2O3.2SiO2 or Al2Si2O5(OH)4 - Hydrated alumina silicate, Pure clay mineral

    China Clay

  • (Materials - Member) Kyanite - Al2O3.SiO2

    Disthene, Cyanite

  • (Materials - Member) Lead Bisilicate Frit - Lead bisilicate frit
  • (Materials - Member) Lead Carbonate - 2PbCO3.Pb(OH)2

    White lead

  • (Materials - Member) Lepidolite - LiF.KF.Al2O3.3SiO2

    Lithium Mica

  • (Materials - Member) Light Magnesium Carbonate - Mg5(CO3)4(OH)2.4H2O

    Hydrated Magnesium Carbonate Mineral, Hydromagnesite, Magnesium Carbonate Light

  • (Materials - Member) Litharge - PbO

    Lead Oxide, Lead(II) oxide, Yellow lead oxide

  • (Materials - Member) Lithium Carbonate - LiCO3

    Lith Carb, Li2CO3

  • (Materials - Member) Manganese Carbonate - MnCO3
  • (Materials - Member) Manganese Dioxide - MnO2

    Mno2, Pyrolusite, Manganese(IV) oxide

  • (Materials - Member) Mullite - 3Al2O3.2SiO2 - Calcined Mullite

    Mulite

  • (Materials - Member) Nepheline Syenite - Generic

    Neph Sy

  • (Materials - Member) Petalite - LiAlSi4O10 or Li2O.Al2O3.8SiO2
  • (Materials - Member) Potash Feldspar - K2O.Al2O3.6SiO2

    K-Feldspar, Orthoclase, K Feldspar, Potassium Feldspar

  • (Materials - Member) Pyrophyllite - Al2O3.4SiO2.H2O - A Soft Hydrous Aluminum Silicate

    Pyrophillite

  • (Materials - Member) Red Lead - Pb3O4

    Minium, Lead(II,IV) oxide

  • (Materials - Member) Rutile - TiO2 - Iron Titanium Mineral
  • (Materials - Member) Silica - SiO2 - Quartz, Flint
  • (Materials - Member) Soda Feldspar - Na2O.Al2O3.6SiO2

    Na-Feldspar, Na Feldspar, Albite

  • (Materials - Member) Sodium Carbonate - Na2CO3 or Na2O.CO2 - The most common form of sodium carbonate

    Soda Ash, Calcined Soda, Anhydrous Sodium Carb, Na2CO3

  • (Materials - Member) Sodium Carbonate Decahydrate - Na2CO3.10H2O

    Washing Soda, Hydrous Sodium Carbonate

  • (Materials - Member) Spodumene - Li2O.Al2O3.4SiO2 or LiAl(Si2O6)
  • (Materials - Member) Strontium Carbonate - SrCO3 or SrO.CO2

    Strontianite

  • (Materials - Member) Talc - Mg3Si4O6 or 3MgO.4SiO2.H2O

    Magnesium Silicate, Steatite, French Chalk, Hydrated talc

  • (Materials - Member) Tin Oxide - SnO2

    Stannic Oxide, Tin(IV) Oxide, Tin Dioxide, SnO2

  • (Materials - Member) Titanium Dioxide - TiO2 - Anatase, Brookite

    TiO2

  • (Materials - Member) Tricalcium Phosphate - Ca3(PO4)2 or 3CaO.P2O5

    Tri-Calcium Phos, Tribasic Calcium Phosphate, Synthetic Bone Ash, Calcium Orthophosphate

  • (Materials - Member) Ulexite - NaCaB5O9·8H2O - Sodium calcium borate

    Television Stone

  • (Materials - Member) Volcanic Ash

    Pumicite

  • (Materials - Member) Wollastonite - CaSiO3 - Calcium Silicate

    Wolastonite

  • (Materials - Member) Zinc Oxide - ZnO - Pure Source Of Zinc

    ZnO, Zincite

  • (Materials - Member) FFF Feldspar - Potash feldspar
  • (Materials - Member) Forshammer Feldspar
  • (Materials - Member) Frit P2963 - Soft alkaline frit

    Potterycrafts Frit P2963

  • (Materials - Member) Frit P3195 - This is actually Ferro Frit 3195

    PotteryCrafts Frit P3195

  • (Materials - Member) Frit P3124

    PotteryCrafts Frit P3124

  • (Materials - Member) Frit P3134 - This is actually Ferro Frit 3134

    PotteryCrafts Frit P3134

  • (Materials - Member) Potclays Frit 2269 - This is actually Ferro Frit 3195
  • (Materials - Member) Potclays Frit 2272 - This is actually Ferro Frit 3124
  • (Materials - Member) Potclays Frit 2273 - This is actually Ferro Frit 3134
  • (Materials - Member) Potclays Frit 2281 - Lead alumina bisilicate frit
  • (Materials - Member) Basalt
  • (Materials) PuraFlow WB Ball Clay - Light burning clay, very plastic Devon Ball Clay

    Black Ball Clay

  • (Materials) PuraFlow AK Ball Clay - Very high plastic buff burning Devon ball clay

    Blue Ball Clay

  • (Materials - Member) Puraflo 50 Kaolin - China clay, Kaolin

    Puraflow 50 China Clay

  • (Materials) BPS Standard Borax Frit - Borax Frit
  • (Materials - Member) Nepheline Syenite Norwegian - Generic

    North Cape Nepheline Syenite




Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()