NotesThese materials are specially defined for makers of crystalline glazes. The decision about what materials to include in this table was a result of a consultation project conducted by John Tilton. Many crystal glazers were consulted.
Remember that INSIGHT can accept a variety of names for a material and still be able to find it in the materials database. This is because materials are defined with names and a list of comma-separated alternate names. This database implements the same feature. For example, the material "Bentone MA" specifies an alternate name of "Macaloid", thus if your glazes specify Macaloid as an ingredient INSIGHT will find Bentone MA and get the chemistry there.
Also, INSIGHT will accept materials into a recipe if they are not in the database, it simply does not include them in the chemistry calculations. For materials like binders, this scheme works well. Notice however that we have included some binders in the database without chemistry information.
There are a few materials in the database that are missing chemistry information (frits). When you generate your MDT (at the MDT download page) you can click a link to immediately see a list of materials and their chemistries, the ones missing oxides should be immediately evident. If you know the chemistry of any of these materials please contact us. Out Bound Links
In Bound Links
- (Materials - Member)
Fusion Frit FZ-647
Frit FZ647, Frit FZ 647
- (Materials)
Alberta Slip - Albany slip substitute
Archie Bray Slip
- (Materials - Member)
Calcined Alumina - Al2O3 - Aluminum oxide
Alumina Calcined, Calcnd Alum, Ground Alumina, Corundum
- (Materials - Member)
Alumina Hydrate - Al2O3.3H2O
Alum Hydrate, Alumina Trihydrate, Hydrated Alumina, Alpha Aluminum Trihydroxide, Gibbsite
- (Materials - Member)
Anhydrous Borax - Na2B4O7 - Fused Borax, Sodium Tetraborate
Calcined Borax, Dehydrated Borax, Pyrobor
- (Materials - Member)
Ball Clay - Highly Plastic Fine Particle Clay
- (Materials - Member)
Barium Carbonate - BaCO3
Barium Carb, Witherite
- (Materials - Member)
Bone Ash - Ca5(OH)(PO4)3
Calcium Phosphate
- (Materials - Member)
Borax Pentahydrate - Na2B4O7.5H2O - Etibor-48
Borax 5 Mol, Sodium Tetraborate, Borax 5-hydrate
- (Materials - Member)
Boric Acid - H3BO3 or B2O3.3H2O
Boracic acid, Orthoboric Acid, Hydrous Boric Oxide
- (Materials - Member)
Calcium Carbonate - CaCO3
Carbonate of Lime, Whiting, Aragonite, Calcite, CaCO3
- (Materials - Member)
Cryolite - Na3AlF6
Cryloite, Sodium Fluoaluminate, Kryolith
- (Materials - Member)
Dolomite - CaCO3.MgCO3 or CaMg(CO3)2 - Double carbonate of magnesia/calcia
Calcium Magnesium Carbonate, Raw Limestone
- (Materials)
Fusion Frit F-75 - Bond Frit
F75 Fusion,Frit F75
- (Materials)
Pemco Frit P-283 - High expansion boron free frit
Frit 283, Frit P283
- (Materials)
G-200 Feldspar - Potash/sodium/calcium 200 mesh Feldspar
G200 Feldspar, G200 Spar, G 200 Spar, G 200, G 200 Feldspar
- (Materials - Member)
Borax Decahydrate - Na2B4O7.10H2O
Sodium TetraBorate Decahydrate, Borax 10-hydrate, 10 Mol Borax, Neobor
- (Materials)
Ceramic Rutile - TiO2
Calcined Rutile, Light Rutile, Rutile Ceramic
- (Materials)
Glomax LL Calcined Kaolin - Calcined Kaolin
Glomax Kaolin, Ajax Glomax Kaolin
- (Materials - Member)
Albany Slip - High iron silty low melting clay
New York Slip, Albany Clay
- (Materials - Member)
Amblygonite - Li.AlF.PO4 - Lithium alumino-fluophosphate
- (Materials - Member)
Australian Spodumene - Li2O.Al2O3.4SiO2
Ausi Spodumene, Ausi Spod
- (Materials)
Bentolite L - White Firing Bentonite
Bentolite
- (Materials - Member)
Bentone EW - Rheological additive for ceramic glazes
- (Materials - Member)
Cobalt Carbonate - CoCO3
Spherocobaltite, CoCO3, Cobalt(II) carbonate
- (Materials - Member)
Cobalt Oxide - CoO
Cobalt(II) oxide, Cobaltosic Oxide, CoO, cobaltous oxide
- (Materials - Member)
Copper Carbonate Basic - CuCO3.Cu(OH)2
Cupric Carbonate, Copper (II) Carbonate, Azurite
- (Materials - Member)
Copper Oxide Black - CuO
Copper (II) Oxide, Black Copper, BCO, Cupric Oxide
- (Materials - Member)
Copper Oxide Red - Cu2O
Cu2O, Red Copper, RCO, Copper (I) Oxide, Cuprous Oxide
- (Materials - Member)
Erbium Oxide
Lanthanide
- (Materials)
A-3 Feldspar - potash feldspar
A3 Feldspar, Kona A-3 Feldspar, Kona A3 Feldspar
- (Materials - Member)
Buckingham Feldspar - Legacy potash feldspar
- (Materials - Member)
Delmonte Feldspar
Del Monte Feldspar
- (Materials - Member)
F-4 Feldspar - Sodium Feldspar
F4 Feldspar, Kona Feldspar, Kona F4, F4 Spar, F 4 Feldspar
- (Materials - Member)
Norfloat Feldspar - Potash feldspar
Norfloat Spar, NORFLOAT Potash Feldspar
- (Materials - Member)
Bayer Frit J-239-P - High sodium boron-free high-expansion frit
Bayer J-239-P
- (Materials - Member)
Degussa Frit 15098 - Frit used in crystalline glazes
- (Materials - Member)
Degussa Frit 90208M
- (Materials - Member)
Degussa Frit 90420M
90420 Zinkbariumfritte
- (Materials - Member)
Ferro Frit 3292 - For Cone 3-5 Sanitary Ware Glazes
F3292
- (Materials - Member)
Ferro Frit 3293
- (Materials - Member)
Ferro Frit 4110 - Leadless high expansion high alkali frit, formerly Frit 3110
Frit KFG 4110
- (Materials - Member)
Fusion Frit F644 - High-sodium boron-free frit
Frit F644
- (Materials - Member)
Fusion Frit 413 - High sodium, boron-free, high expansion frit
- (Materials - Member)
Fusion Frit 435 - Boron free frit
Frit 435, Fusion Frit F-435
- (Materials - Member)
Fusion Frit FZ-583 - Barium Zinc Zero Boron frit
Frit FZ583
- (Materials - Member)
Heraeus Schauer Frit K 1562 - Lead sodium zero alumina frit
- (Materials - Member)
Heraeus Schauer Frit K 1325 - High-sodium low alumina frit
Frit K1325
- (Materials - Member)
Heraeus Schauer Frit K 3066 - Lead sodium zero alumina frit
- (Materials - Member)
Mondre and Manz Frit 1233
Alkalifritte C-1233, Alkalifritte M 1233
- (Materials - Member)
Mondre and Manz Frit 4067 - Barium zinc potash low alumina leaded frit
- (Materials - Member)
Gerstley Borate - Plastic Calcium Borate
Colemanite, Calcium Borate, Borocalcite
- (Materials - Member)
Grolleg Kaolin - Fine White Burning English Kaolin, English China Clay
Grolleg China Clay
- (Materials - Member)
Iron Chromate - FeO.Cr2O3
Ferric Chromate, Chromite, Chromate of Iron
- (Materials - Member)
Iron Oxide Black - Fe3O4 - Ferrous ferric oxide, Synthetic Magnetite
Fe3O4, Black Iron Oxide, BIO, Magnetite Powder, Iron(II,III) Oxide
- (Materials - Member)
Molochite - Highly Calcined Alumina Silicate
- (Materials - Member)
Molybdenum Trioxide - MoO3
- (Materials - Member)
Molybdenum Disulfide - MoS2
- (Materials - Member)
Praseodymium Oxide
Lanthanide oxide
- (Materials - Member)
Neodymium Oxide
Lanthanide
- (Materials - Member)
Nickel Oxide Green - NiO
NiO, Nickelous oxide, Green Nickel Oxide
- (Materials - Member)
Nickel Oxide Black - Ni2O3
Ni2O3, Nickelic Oxide, Nickel sesquioxide, Nickel (II) oxide
- (Materials - Member)
Nickel Carbonate - NiCO3
NiCO3
- (Materials - Member)
Nytal Talc - Hydrous Magnesium Calcium Silicate
- (Materials - Member)
Nepheline Syenite Norwegian - Generic
North Cape Nepheline Syenite
- (Materials - Member)
Redart - Red Firing Earthenware
Red Art
- (Materials - Member)
Silver Nitrate - AgNO3
AgNO3
- (Materials - Member)
Silver Chloride - AgCl
- (Materials - Member)
Silver Phosphate - Ag3PO4
- (Materials - Member)
Tungsten Sulfide - WS2
Tungsten(IV) Sulfide
- (Materials - Member)
Tungsten Trioxide - WO3
Tungsten(VI) oxide, Tungsten Oxide
- (Materials - Member)
Triuranium Octaoxide - U3O8
Yellowcake, Uranium Oxide
- (Materials - Member)
Uranyl Nitrate - UO2(NO3)2
- (Materials - Member)
Vanadium Pentoxide - V2O5
Vanadium (V) Oxide
- (Materials - Member)
Veegum - Glaze Hardener, Binder
Veegum T, Veegum CER, Veegum Pro
- (Materials - Member)
Yellow Ochre - High iron clay
Hydrated ferric oxide
- (Materials - Member)
Zircopax - Zirconium Silicate
- (Materials - Member)
Flint - SiO2 - Silica
- (Materials - Member)
Bentone MA - Glaze Suspender, Hectorite
Macaloid
- (Materials - Member)
Pearl Ash - K2CO3
Potassium Carbonate, K2CO3, Pearlash
- (Materials - Member)
Bentonite
Montmorillonite
- (Materials - Member)
Colemanite - 2CaO.3B2O3.5H2O or CaB3O4(OH)3·H2O
- (Materials - Member)
Cornwall Stone
Cornish Stone, China Stone, Corn Stn, China-stone
- (Materials - Member)
Fluorspar - CaF2
Fluorite, Calcium Fluoride, Blue John
- (Materials - Member)
Ilmenite - FeTiO3 or FeO.TiO2 - Iron & Titanium Oxide
Illmenite, Ferrous Titanate, Iron Titanate
- (Materials - Member)
Iron Oxide Red - Fe2O3 - Synthetic Hematite
Ferric Oxide, Red Iron Oxide, RIO, Iron(III) oxide, Fe2O3, Hematite
- (Materials - Member)
Iron Oxide Yellow - FeO.OH or Fe2O3.H2O - Fe2O3.H2O, FeO(OH), Goethite
Iron(III) oxide, hydrated iron oxide, iron(III) hydroxide
- (Materials - Member)
Lead Bisilicate Frit - Lead bisilicate frit
- (Materials - Member)
Lead Monosilicate Frit
- (Materials - Member)
Lepidolite - LiF.KF.Al2O3.3SiO2
Lithium Mica
- (Materials - Member)
Lithium Carbonate - LiCO3
Lith Carb, Li2CO3
- (Materials - Member)
Manganese Carbonate - MnCO3
- (Materials - Member)
Manganese Dioxide - MnO2
Mno2, Pyrolusite, Manganese(IV) oxide
- (Materials - Member)
Nepheline Syenite - Generic
Neph Sy
- (Materials - Member)
Potash Feldspar - K2O.Al2O3.6SiO2
K-Feldspar, Orthoclase, K Feldspar, Potassium Feldspar
- (Materials - Member)
Red Lead - Pb3O4
Minium, Lead(II,IV) oxide
- (Materials - Member)
Silica - SiO2 - Quartz, Flint
- (Materials - Member)
Sodium Carbonate - Na2CO3 or Na2O.CO2 - The most common form of sodium carbonate
Soda Ash, Calcined Soda, Anhydrous Sodium Carb, Na2CO3
- (Materials - Member)
Spodumene - Li2O.Al2O3.4SiO2 or LiAl(Si2O6)
- (Materials - Member)
Strontium Carbonate - SrCO3 or SrO.CO2
Strontianite
- (Materials - Member)
Talc - Mg3Si4O6 or 3MgO.4SiO2.H2O
Magnesium Silicate, Steatite, French Chalk, Hydrated talc
- (Materials - Member)
Tin Oxide - SnO2
Stannic Oxide, Tin(IV) Oxide, Tin Dioxide, SnO2
- (Materials - Member)
Titanium Dioxide - TiO2 - Anatase, Brookite
TiO2
- (Materials - Member)
Wollastonite - CaSiO3 - Calcium Silicate
Wolastonite
- (Materials - Member)
Zinc Oxide - ZnO - Pure Source Of Zinc
ZnO, Zincite
- (Materials)
Ceramitalc - Talc
- (Materials)
Custer Feldspar - Potash Feldspar
Custer Spar
- (Materials)
EP Kaolin - Plastic White Firing Kaolin
EPK, Edgar Plastic Kaolin, EPK Kaolin
- (Materials)
Eureka Feldspar - Legacy low calcium potash feldspar
- (Materials)
Ferro Frit 3110 - High alkali, low alumina and boron leadless high expansion frit
F3110, Frit KFG 4110, Ferro Crystal Frit
- (Materials)
Ferro Frit 3124 - Leadless high calcium borosilicate frit
F3124
- (Materials)
Ferro Frit 3134 - Leadless and zero alumina high calcia borosilicate frit
F3134
- (Materials)
Ferro Frit 3195 - Leadless High Borax/calcia for glaze
F3195
- (Materials)
General Frit GF-106 - High-sodium high expansion frit
Frit 106, Frit GF106, GF 106, GC 106,Frit GF-106
- (Materials)
Pemco Frit P-25 - Leadless alkaline fluorine frit, use for cone 06-02
Pemco 25, Pemco Frit 25
- (Materials)
Kingman Feldspar - Potash Feldspar
- (Materials)
NC-4 Feldspar
NC4 Feldspar, Spruce Pine #4 Spar
- (Materials)
OM #4 Ball Clay - Tennessee Ball Clay
OM4 Ball Clay, OM4, OM#4, OM 4, Old Mine #4, OM-4 Ball Clay
- (Materials)
Pioneer Kaolin - Medium plasticity kaolin
Georgia Kaolin
- (Materials)
Tile #6 Kaolin - Highly Plastic Fine Grained
Tile 6, Tile#6 Kaolin
- (Materials)
Oxford Feldspar - Potash Feldspar
- (Materials - Member)
Copper Carbonate - CuCO3
Synthetic Malachite, CuCO3
- (Materials - Member)
Chrome Oxide - Cr2O3
Chromium (III) Oxide, Cr2O3, Chromium Oxide
- (Materials)
VanTalc - Hydrous Magnesium Calcium Silicate
- (Materials)
Degussa Frit 90378
- (Materials)
Degussa Frit 90208
- (Materials)
Degussa Frit 90205
90205 Bleiborsilikat
- (Materials)
Degussa Frit 90191
90191 Alkaliborfritte
- (Materials)
Degussa Frit 90187
- (Materials)
Degussa Frit 90176
- (Materials)
Degussa Frit 90158
90158 Natriumborsilikat
|