Digitalfire Ceramic Materials Database | Logged in as Level 2 access: Logout |
Oxides | Minerals | Materials | Recipes | Articles | Glossary | Hazards | Library | MDT | Pictures | Properties | Schedules | Temperatures | Tests | Troubles | Typecodes
Chemistry %
|
Out Bound Links
F4 Feldspar, Kona Feldspar, Kona F4, F4 Spar, F 4 Feldspar
Na-Feldspar, Na Feldspar, Albite
The decision about what materials to include in th...
We are working on this database and would apprecia...
We are working on this database and would apprecia...
<?xml version="1.0" encoding="UTF-8"?> <material name="Unispar 50" descrip="Soda Feldspar" searchkey="Unispar-50" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.700" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="19.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.040" tolerance=""/> </oxides> </material>
|
Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved |
|
INSIGHT is ceramic chemistry |