Digitalfire Ceramic Materials Database

Logged in as Level 2 access: Logout


Plastic Vitrox

White Burning Plastic Feldspar

Chemistry %

CaO1.00
MgO0.50
K2O5.00
Na2O0.90
TiO20.10
Al2O312.70
SiO276.50
Fe2O30.50
 

Volatiles %

LOI2.80

See PV Clay.

Richard Willis

A California feldspathic earth, usually packaged under the label PVC for “Plastic Vitrox Clay”, that is similar in makeup to Cornwall Stone but fires whiter. It is preferred by many for use in white clay or glaze formulas where kaolin or a “white clay” is called for.
Typical empirical analyses are SiO2 75.56%, Al2O3 14.87%, Fe2O3 0.09%, CaO 0.22%, MgO 0.20%, Na2O 0.29%, K2O 6.81% and CaO 1.00%, K2O 5.00%, MgO 0.50%, Na2O 0.90%, TiO2 0.10%, Al2 >O3 12.70%, SiO2 76.50%, Fe2O3 0.50%
A well-behaved casting slip for cone 8 or lower can be made of 1 part PV to 3 parts talc and 2 parts ball clay. A simple cone 6 glaze can be made of 1 part PV to 1 part borocalcite (2CaO.3B2O3.5H2O).

Out Bound Links

In Bound Links


Pictures
PV Clay fired from cone 7-11 oxidation and 10 reduction.


XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?>
<material name="Plastic Vitrox" descrip="White Burning Plastic Feldspar" searchkey="PV Clay, Plas Vitrox" loi="0.00" casnumber="12168-80-8">
<oxides>
<oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.000" tolerance=""/>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.000" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.900" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.100" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.700" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="76.500" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.500" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="LOI" name="Loss on Ignition" percent="2.800" tolerance=""/>
</volatiles>
</material>



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()