Kentucky #6

Kentucky Ball Clay

Chemistry %

CaO0.30
MgO0.30
K2O0.60
Na2O0.10
TiO22.10
Al2O323.60
SiO263.90
Fe2O30.90
 

Volatiles %

LOI8.20
PCE - Pyrometric Cone Equivalent 29-31

Out Bound Links

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?>
<material name="Kentucky #6" descrip="Kentucky Ball Clay" searchkey="" loi="0.00" casnumber="70694-09-6">
<oxides>
<oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.600" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="2.100" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="23.600" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.900" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.900" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="LOI" name="Loss on Ignition" percent="8.200" tolerance=""/>
</volatiles>
</material>



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()