Gresan C Ball Clay

REFINED NOODLED BALL CLAY

Chemistry %

CaO0.20
MgO0.30
K2O2.20
Na2O0.30
TiO21.50
Al2O324.30
SiO263.10
Fe2O30.90
 

Volatiles %

C0.60
LOI7.20

PARTICLE SIZE (E.S.D.)
%> %< %< %<
125u 10u 2u 1u
0.05 92 68 58


Out Bound Links

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?>
<material name="Gresan C Ball Clay" descrip="REFINED NOODLED BALL CLAY" searchkey="" loi="7.80" casnumber="70694-09-6">
<oxides>
<oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.200" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.300" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.500" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="24.300" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.100" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.900" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="C" name="Carbon" percent="0.600" tolerance=""/>
<volatile symbol="LOI" name="Loss on Ignition" percent="7.200" tolerance=""/>
</volatiles>
</material>



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()