The number of different frits in the world can be intimidating, there are thousands. However, unlike stains, their are a wide range of standard formulations that have been made for many years. We are having difficulty finding and classifying them all and it will be done in time.
Obviously, since color and other fired properties are a product of the chemistry, we need to know the chemistry of the frits we use to fully control and understand them. Actually, if we have the chemistry, all other information is secondary. However many frits have specific chemistries that are the product of an intense research effort to produce a specific result using a specific firing method. To anyone other than the engineers to developed the frit, the chemistry will only seem novel. Such a frit can obviously just be used to supply oxides to a glaze as any other material, but it purpose (and likely its greater cost) would be wasted.
Unfortunately most frit companies either do not publish chemistry information at all (some have in the past but have discontinued) or publish approximate chemistries. Frit manufacturers often do reveal chemistries to individual users. Thus old product literature, books, substitution information, xray diffraction or other means of analysing the chemistry, leaked information from technical people at manufacturers and derivation by comparison of approximate chemistries to standard formulations of other producers are the sources for the numbers provided here. Fast-fire and other special purpose frits are a more recent development and the chemistry of these is more closely guarded. If you have any frit data, please contact us so we can share it. As you can see we do not have advertising on this site, we have always striven to share this type of information with a good motive. In future we will be providing better tools to search for frit substitutes and find frits based on their chemistry.
In the curious world of frits, the websites of most frit producers offer surprisingly little information about their products, generally most of the documentation we have comes from users and authors. Some companies do not even have websites or pages that google can find. Many companies change the names of their products over time, this adds to the complexity of maintaining chemistry info. In addition, suppliers often buy frits from a manufacturer, then rename and sell under their own brand (fortunately often the names bear some resemblance to the original so these can be tracked). Other companies number the same frit differently in different countries. Much of the information about specific frits is wrong or outdated, but we can only use what we have until we can convince the manufacturers to be more open. If the chemistry of a frit is not available here, often there will be a link to an equivalent (keep in mind that links are classified so a link to a substitute is not equivalent to a link to a similar one). Our INSIGHT software has a mechanism for naming a frit one way and using the chemistry of another.
Two key frit properties are the thermal expansion and melting behavior (remember that frits do not melt at a specific temperature but over a range). There are different ways of measuring both of these and we are attempting to document these in the testing section. It is generally more practical only to compare the numbers of products from the same manufacturer.
The particle size of frits is not nearly as important as it is for stains. There is a wide range of qualities of frits available (again quality generally refers to consistent particle dynamics and chemistry). The manufacturers using older equipment and processing methods have greater problems maintaining quality. Other companies have modern equipment but have not fully learned the importance of quality, sometimes a supplier will act as an agent (and even blender) between a manufacturer and users to assure quality.
The production of stains can entail the usage of often toxic materials and money can be saved by taking shortcuts it dealing with wastes. Some manufacturers are taking advantage of less stringent environmental and workplace hazard regulations in third world countries to produce stains cheaper but sometimes with greater human cost to the local people and their land.
See Also
- FRFU - Frit Fusibility Test
- HMA - Heating Microscope Analysis for Frits
- FTP - Frit Transformation Point
- A Low Cost Tester of Glaze Melt Fluidity
This device to measure glaze melt fluidity helps you better understand your glazes and materials and solve all sorts of problems.
- The Chemistry, Physics and Manufacturing of Glaze Frits
A detailed discussion of the oxides and their purposes, crystallization, phase separation, thermal expansion, solubility, opacity, matteness, batching, melting.
- Glaze Types, Formulation and Application in the Tile Industry
An technical overview of various glaze type used in the tile industry along with consideration of the materials, processes and firing.
- Low Budget Testing of the Raw and Fired Properties of a Glaze
There is more to glazes than their visual character, they have other physical properties like hardness, thermal expansion, leachability, chemistry and they exhibit many defects. Here are some simple tests.
- Lead in Frits: The Hazards
- UnDescribed - Frit
A ceramic glass that has been premixed from raw powdered minerals and then melted, cooled by quenching in water, and ground into a fine powder. Huge quantities and varieties of frits are manufactured for the ceramic industry every year (especially for tile) by dozens of different companies.
Althoug...
- Borax Frit, Boron Frit
This term is very generic, referring of course to frits that contain boron. Unfortunately that is 80-90% of available frits! Boron frits may have 1% boron or 50% boron. Even though the boron in the frit is no longer in the borax form it is still customary to refer to such as "borax frits". Since man...
Frits
- Bayer Frit J-239-P
High sodium boron-free high-expansion frit
- Blyth Frit 3104
- Ceradel Frit 3110
High sodium, low boron/alumina frit
- Ceradel Frit 3134
High calcia borosilicate frit
- Ceradel Frit 3195
Low temperature glaze
- Ceradel Frit C 1249
Lead bisilicate frit, Bisilicate de plomb
- Ceradel Frit C 1250
Lead bisilicate frit, Bisilicate de plomb
- Ceradel Frit C 1251
Lead monosilicate frit, Monosilicate de plomb
- Ceradel Frit C 1252
Fritte borocalcique sans plomb
- Ceradel Frit C 1253
High expansion frit, Fritte boro-alcaline sans plomb
- Ceradel Frit C 1254
Lead monosilicate frit, Frit calco-alcaline sans plomb
- Ceradel Frit C 1255
Fritte zirconifere sans plomb, low expansion ziron frit
- Ceradel Frit C 1256
Fritte borique, very low expansion borate frit
- Chrysanthos Frit FR001
Zinc zircon white opaque frit
- Chrysanthos Frit FR002N
Low expansion transparent frit
- Chrysanthos Frit FR003
High expansion alkali frit
- Chrysanthos Frit FR004
Alumina lead bisilicate frit
- Chrysanthos Frit FR005
High boron sodium frit
- Chrysanthos Frit FR006
High calcium borosilicate frit
- Colorobia Frit F4
- Colorobia Frit F5
- Degussa Frit 15098
Frit used in crystalline glazes
- Degussa Frit 90001
- Degussa Frit 90016
- Degussa Frit 90062
- Degussa Frit 90142
- Degussa Frit 90155
- Degussa Frit 90158
- Degussa Frit 90167
High alkali borosilicate frit
- Degussa Frit 90176
- Degussa Frit 90187
- Degussa Frit 90191
- Degussa Frit 90198
Leadless high alkali borosilicate frit
- Degussa Frit 90205
- Degussa Frit 90208
- Degussa Frit 90208M
- Degussa Frit 90226
- Degussa Frit 90242
- Degussa Frit 90321
- Degussa Frit 90328
- Degussa Frit 90352
- Degussa Frit 90368
- Degussa Frit 90378
- Degussa Frit 90420M
- Douteux Frit LB75
- Ferro Frit 1012
Calcium borosilicate frit
- Ferro Frit 1057
Leadless calcium borosilicate frit
- Ferro Frit 1077
Calcium borosilicate frit
- Ferro Frit 1081
Insoluble colemanite substitute
- Ferro Frit 1085
Dense zircon white frit
- Ferro Frit 114
- Ferro Frit 1212
Alkali borosilicate frit
- Ferro Frit 210R
- Ferro Frit 221-201
- Ferro Frit 2244
Calcium borosilicate frit
- Ferro Frit 271D
Clear cone 6 dinnerware glaze frit
- Ferro Frit 2954
Calcium borosilicate frit
- Ferro Frit 3043
Netherland, Flanders area (Ferro?)
- Ferro Frit 3110
High alkali, low alumina and boron leadless high expansion frit
- Ferro Frit 3124
Leadless high calcium borosilicate frit
- Ferro Frit 3127
- Ferro Frit 3134
Leadless and zero alumina high calcia borosilicate frit
- Ferro Frit 3185
Low melting alkali borate bonding frit for abrasives
- Ferro Frit 3191
A source of alkali borate intended for use in abrasives indust
- Ferro Frit 3193
Alkaline borate bonding frit for abrasive industry
- Ferro Frit 3195
Leadless High Borax/calcia for glaze
- Ferro Frit 3210
- Ferro Frit 3211
Calcium Borate Frit
- Ferro Frit 3221
Leadless alkali borosilicate frit
- Ferro Frit 3223
- Ferro Frit 3224
Alkali borosilicate frit
- Ferro Frit 3225
Low expansion cone 04 frit for vitrified bonded abrasives
- Ferro Frit 3226
Leadless vitrified bonded abrasives frit
- Ferro Frit 3227
For low temperature vitreous bonding in metals industry
- Ferro Frit 3230
Very high alkaline frit for copper blue, manganese purples
- Ferro Frit 3234
- Ferro Frit 3240
Zinc barium artware and tile glaze frit
- Ferro Frit 3247
Leadless very high barium boron free frit
- Ferro Frit 3248
Leadless calcium potassium borosilicate frit
- Ferro Frit 3249
Low expansion leadless magnesia borosilicate frit
- Ferro Frit 3257
Very high barium artware frit
- Ferro Frit 3264
Leadless high sodium borosilicate
- Ferro Frit 3269
Leadless Sodium Boron Frit
- Ferro Frit 3270
Borosilicate cone 06-04 frit for cobalt colors
- Ferro Frit 3271
Leadless calcium borosilicate frit
- Ferro Frit 3275
Custom frit for glass bonded mica
- Ferro Frit 3276
- Ferro Frit 3278
Leadless high boron alkali silicate frit
- Ferro Frit 3280
Used in custom vitrified bonded abrasives.
- Ferro Frit 3281
- Ferro Frit 3284
Frit for satin matte tile glazes
- Ferro Frit 3286
Strontium fluxed all fritted leadless clear glaze
- Ferro Frit 3288
Sodium calcium borosilicate frit for wall tile glazes
- Ferro Frit 3289
High barium leadless frit for bright colors, satin finishes
- Ferro Frit 3291
Magnesia frit for vitrified bonded abrasives
- Ferro Frit 3292
For Cone 3-5 Sanitary Ware Glazes
- Ferro Frit 3293
- Ferro Frit 3299
- Ferro Frit 3300
Medium lead high zinc glaze for for cone 02-8
- Ferro Frit 3302-D
Opaque frit for white and pastel glazes cone 04-06
- Ferro Frit 3304
High lead zincless frit for clear glaze cone 04-08
- Ferro Frit 3327
Lead monosilicate frit
- Ferro Frit 3336
Zircon cone 04-05 frit
- Ferro Frit 3337
- Ferro Frit 3377 - PbO.SiO2
Lead:silica 1:1 ration frit
- Ferro Frit 3379
Lead silicate frit
- Ferro Frit 3386
Medium lead borosilicte for cone 010-5
- Ferro Frit 3396
Lead alkali frit
- Ferro Frit 3403
Lead alumina bisilicate frit
- Ferro Frit 3417
Leaded frit for all fritted glazes cone 06-01
- Ferro Frit 3419
High lead borosilicate glaze frit cond 08-02
- Ferro Frit 3435
Low lead low alumina calcium borosilicate frit
- Ferro Frit 3438
- Ferro Frit 3441
- Ferro Frit 3442
- Ferro Frit 3446
- Ferro Frit 3447
Barium lead calcuim borosilicate frit
- Ferro Frit 3451
- Ferro Frit 3453
Lead monoborate frit
- Ferro Frit 3454
Low lead borate frit
- Ferro Frit 3455
- Ferro Frit 3456
- Ferro Frit 3457
Leaded calcium boron free frit
- Ferro Frit 3458
Low lead calcium borate frit
- Ferro Frit 3462
- Ferro Frit 3463
- Ferro Frit 3464
- Ferro Frit 3465
Low lead high borax frit cone 08-02
- Ferro Frit 3466
Low lead, low boron, low alumina glaze frit cone 2-7
- Ferro Frit 3467
Low Lead High Alumina Glaze Frit
- Ferro Frit 3470
High lead zinc frit for artware and hobby glazes
- Ferro Frit 3471
Leaded barium calcium borosilicate frit
- Ferro Frit 3476
High lead borosilicate frit
- Ferro Frit 3480
- Ferro Frit 3481
Medium lead calcium cone 06-02 frit for chrome tin colors
- Ferro Frit 3482
Medium lead high titanium glaze frit cone 06-02
- Ferro Frit 3485
Medium lead sodium borosilicate frit
- Ferro Frit 3487
Low lead high calcium frit cone 01-3
- Ferro Frit 3489
Lead bisilicate frit with 5% CaO
- Ferro Frit 349
Low Lead Frit
- Ferro Frit 3490
High Lead Frit
- Ferro Frit 3493
Medium lead zincless hobby artware cone 06-04 glaze frit
- Ferro Frit 3494
- Ferro Frit 3496
Medium lead zincless for cone 04-2 artware glazes
- Ferro Frit 3497
Medium lead zincless frit cone 2-5
- Ferro Frit 3498
Lead alumina bisilicate
- Ferro Frit 3499
- Ferro Frit 3509
Low lead calcium silicate frit
- Ferro Frit 3516
Lead calcium borosilicate frit
- Ferro Frit 3519
Lead zinc borosilicate frit
- Ferro Frit 3528
- Ferro Frit 3532
- Ferro Frit 3536
- Ferro Frit 3541
- Ferro Frit 3545
Leaded calcium borosilicate frit
- Ferro Frit 3548
High lead cadmium bearing frit cone 013-07
- Ferro Frit 3552
Low lead zinc frit for cone 02-2
- Ferro Frit 3560
Very low lead zinc barium frit
- Ferro Frit 3563
LEAD BEARING FRIT
- Ferro Frit 3565
Low lead calcium borosilicate cone 01-5 glaze frit
- Ferro Frit 3576
Medium lead hobby/artware glaze frit cone 06-04
- Ferro Frit 3600
High lead cadmium frit for red/yellow artware glazes cone 010-03
- Ferro Frit 3602
Lead alumina bilsilicate frit
- Ferro Frit 3620
- Ferro Frit 3626
Lead bisilicate frit
- Ferro Frit 3813
- Ferro Frit 3814
Leadless calcium borosilicate frit
- Ferro Frit 3819
Leadless high sodium frit for cone 06-02
- Ferro Frit 3820
Zinc alkali borosilicate frit
- Ferro Frit 3824
Leadless zinc frit
- Ferro Frit 3831
Barium calcium alkali boron free frit
- Ferro Frit 3833
Filler for resin bonded abrasives
- Ferro Frit 3834
Filler for resin bonded abrasives
- Ferro Frit 3838
Filler for resin bonded abrasives
- Ferro Frit 3846
Antimony opacified, high expansion frit
- Ferro Frit 3851
High magnesia leadless boron-free low expansion frit
- Ferro Frit 3878
- Ferro Frit 3898
- Ferro Frit 4049
High boron low lead frit
- Ferro Frit 4064
Lead alumina bilsilicate frit with small amount of sodium
- Ferro Frit 4101
High expansion sodium borosilicate fluorine frit
- Ferro Frit 4103
Zinc bearing borosilicate frit
- Ferro Frit 4108
Low alumina high CaO boro silicate frit
- Ferro Frit 4110
Leadless high expansion high alkali frit, formerly Frit 3110
- Ferro Frit 4112
Calcium Borate Frit
- Ferro Frit 4113
General purpose hard and versatile boron frit
- Ferro Frit 4124
Hard boric oxide frit
- Ferro Frit 4125
Low melting high expansion sodium borosilicate fluorine frit
- Ferro Frit 4144
Australian equivalent of Frit 3134
- Ferro Frit 4193
Transparent hard barium zinc borosilicate leadless frit
- Ferro Frit 4194
Soft sodium borosilicate frit
- Ferro Frit 4346
IRON FRIT
- Ferro Frit 4364
Lead alumina bilsilicate frit
- Ferro Frit 4396
Netherland, Flanders area (Ferro?)
- Ferro Frit 4616
High zinc borosilicate frit for matte glazes 1040-1100C
- Ferro Frit 4712
Borosilicate hard clear general purpose frit 1040-1100C
- Ferro Frit 530
High expansion sodium borosilicate fluorine frit
- Ferro Frit 5301
High Expansion Leadless Fluorine Frit
- Ferro Frit 5325P
Soft sodium borosilicate frit
- Ferro Frit 9102
Dense zircon white frit
- Ferro Frit 9146
Dense zircon white frit
- Ferro Frit 938
Transparent hard barium zinc borosilicate leadless frit
- Ferro Frit CC-233
NO LEAD ZIRCONIUM
- Ferro Frit CC-250
Clear fast fire cone 06 glaze frit with 10% kaolin
- Ferro Frit CC-251
Floor tile glazes
- Ferro Frit CC-252
Custom frit for spark plugs
- Ferro Frit CC-253
Custom frit for resistor plugs
- Ferro Frit CC-254
FLOOR TILE GLAZE FRIT
- Ferro Frit CC-257
High Barium Frit
- Ferro Frit CC-257-2
Strontium Frit
- Ferro Frit CC-261
Zinc frit
- Ferro Frit CC-262
- Ferro Frit CC-263
GLAZE FRIT CONE 04-2
- Ferro Frit CC-265
- Ferro Frit CC-266
- Ferro Frit CC-270
- Ferro Frit CC-274
- Ferro Frit CC-277
- Ferro Frit CC-279
Clear cone 06-04 frit
- Ferro Frit CC-411
- Ferro Frit CC-657
Low zinc calcium borate frit
- Ferro Frit CL-408
- Ferro Frit CM-887
- Ferro Frit CM-895
- Ferro Frit CM-943
- Ferro Frit CM-944
- Ferro Frit CZ-102
- Ferro Frit CZ-105
Zircon frit for partially fritted tile glazes
- Ferro Frit CZ-106
- Ferro Frit FB-145-G
Vitrified bonded abrasives frit
- Ferro Frit FB-149B
Cone 07-04 transparent crackle (high expansion) frit
- Ferro Frit FB-175-L
- Ferro Frit FB-179-G
Cadmium leaded frit for red/yellow hobby and artware glazes
- Ferro Frit FB-208-L
- Ferro Frit FB-250-L
Vitrified bonded abrasives frit
- Ferro Frit FB-258-A
FeMn frit, flux color
- Ferro Frit FB-276-P
Artware Glaze Frit
- Ferro Frit FB-280-L
CUSTOM DIAMONITE FRIT
- Ferro Frit FB-282-B
Zircon frit for partially fritted opaque tile glazes
- Ferro Frit FB-282-O
Vitrified bonded abrasives frit
- Ferro Frit FB-284-M
Barium Frit
- Ferro Frit FB-285-D
Leaded frit for use in matte glazes
- Ferro Frit FB-286-D
- Ferro Frit FB-288-A
- Ferro Frit FB-288-D
Frit for fritted satin matt glazes
- Ferro Frit FD-276-P
- Ferro Frit R-1
Bonding frit
- Ferro Frit R-210M
- Ferro Frit Z-119
- Frit 1047
High magnesia borosilicate frit
- Frit 1078
Soft sodium borosilicate frit
- Frit 1201
High zinc high potash high boron low silica frit
- Frit 1202
Alkali high calcium low boron low alumina frit
- Frit 1203
Alkali calcium very low boron alumina silicate frit
- Frit 1209
Calcium borate frit with very low alumina, silica
- Frit 1210
Zinc alkali opacified alumina silicate frit
- Frit 1213
Barium iron borosilicate low alumina frit
- Frit 1214
Barium manganese borosilicate low alumina frit
- Frit 1451
Netherlands, Flanders area (Ferro?)
- Frit 1510
Netherland, Flanders area (Ferro?)
- Frit 1817
High alkali leadless aluminun silicate frit
- Frit 1818
Alkali calcium aluminun silicate frit
- Frit 1843
Lead borosilicate frit
- Frit 2120
High sodium aluminum silicate frit
- Frit 268-D
Zircon unleadled frit
- Frit 282-b
- Frit 288-B
- Frit 2958
Netherlands, Flanders area (Ferro?)
- Frit 2963
Netherlands, Flanders area (Ferro?)
- Frit 3069P
High boron frit
- Frit 3221
Calcium borate
- Frit 439
Gerstley Borate Substitute
- Frit 45301
Sodium borosilite for cadmium selenium glazes
- Frit 5151
IRON FRIT
- Frit 6004
Israel
- Frit A3249/p
- Frit B300
Lead alumina bilsilicate frit
- Frit FA-233
ZIRCON WHITE LEADLESS FRIT
- Frit FNO 143
- Frit FR-170A
Opaque white glaze frit cone 06-04
- Frit G-23
LEADED FRIT
- Frit G-24
LEADED FRIT
- Frit HP33
- Frit J
Danish frit
- Frit LP891
- Frit MOK 1
- Frit NR 2
- Frit P2950
Lead alumina bilsilicate frit
- Frit P2952
BORAX FRIT
- Frit P2953
Borax frit
- Frit P2954
Calcium Borate Frit similar to Gerstley Borate
- Frit P2955
High alkali low alumina borax frit
- Frit P2957
Low expansion borax frit
- Frit P2960
Low Expansion Frit
- Frit P2961
Standard alkaline frit
- Frit P2962
High alkaline frit
- Frit P2963
Soft alkaline frit
- Frit P3110
This is actually Ferro Frit 3110
- Frit P3124
- Frit P3134
This is actually Ferro Frit 3134
- Frit P3195
This is actually Ferro Frit 3195
- Frit PC-4C-74
- Frit RCG 2430
- Frit V-3
- Frit Welte FR 2010 - PbO.SiO2
Lead:silica 1:1 ration frit
- Frit Welte FR 2015 - PbO.2SiO2
Lead bisilicate frit
- Frit Welte FR 2020 - PbO.B2O3.2SiO2
Lead bisilicate monoborate frit
- Frit Welte FR 2025
Lead borate frit
- Frit XF-150
Custom refractory component frit
- Fusion Frit 294
Magnesium frit
- Fusion Frit 413
High sodium, boron-free, high expansion frit
- Fusion Frit 435
Boron free frit
- Fusion Frit 5325
Low melting high expansion sodium borosilicate frit
- Fusion Frit 556
Zinc matte frit for fast fire
- Fusion Frit 565
Zinc frit
- Fusion Frit 578
Strontium barium frit
- Fusion Frit 587
Opaque frit
- Fusion Frit 605
Zinc free calcium frit
- Fusion Frit F-02
Zinc free calcium frit
- Fusion Frit F-05
Strontium barium frit
- Fusion Frit F-10
Opacified flux for cone 1 tile glazes
- Fusion Frit F-102
- Fusion Frit F-105
Alkali boron flux for wall tile
- Fusion Frit F-12
Artware Flux Calcium Frit
- Fusion Frit F-125
Wall Tile Opaque Frit
- Fusion Frit F-13
Fast Fire Calcium Frit
- Fusion Frit F-134
Strontium frit base for cone 5-6 glazes
- Fusion Frit F-145
Alkaline magnesia boron frit
- Fusion Frit F-15
Low expansion frit
- Fusion Frit F-175
Barium sodium zirconium frit
- Fusion Frit F-18
Dinnerware Strontium Frit
- Fusion Frit F-19
Boro Calcium Dinnerware Frit
- Fusion Frit F-2
High Calcium Boron Leadless
- Fusion Frit F-215
- Fusion Frit F-225
Leadless Sodium Boron Frit
- Fusion Frit F-237
- Fusion Frit F-245
Alkali boron bonding frit
- Fusion Frit F-26
Strontium baruim frit
- Fusion Frit F-280
- Fusion Frit F-300
Strontium frit for sanitaryware
- Fusion Frit F-304
- Fusion Frit F-309
Calcium borate frit, Gerstley Borate substitute
- Fusion Frit F-310
- Fusion Frit F-326
Opaque frit
- Fusion Frit F-34
High boron zinc free calcium frit
- Fusion Frit F-359
- Fusion Frit F-367
Bond Frit
- Fusion Frit F-38
Strontium Flux
- Fusion Frit F-380
Barium leadless frit
- Fusion Frit F-390
- Fusion Frit F-395
- Fusion Frit F-403
Barium matte opaque frit
- Fusion Frit F-43
Alkaline boron flux for high temperature glazes
- Fusion Frit F-49
Opacified frit for fast fire tiles
- Fusion Frit F-492
High boron low expansion flux
- Fusion Frit F-493
High lithium frit
- Fusion Frit F-495
Calcium borate dinnerware frit
- Fusion Frit F-496
Clear Alkali Boron Frit
- Fusion Frit F-499
High sodium boron frit
- Fusion Frit F-502
Strontium barium frit
- Fusion Frit F-506
Strontium dinnerware frit
- Fusion Frit F-520B
Calcium borate dinnerware frit
- Fusion Frit F-524
Low fire base glaze, add 10% kaolin, adjust with other frits
- Fusion Frit F-537
Zinc free calcium frit
- Fusion Frit F-541
Fast fire opaque frit
- Fusion Frit F-562
Alkali boron frit
- Fusion Frit F-567
Alkali boron frit
- Fusion Frit F-577
Calcium magnesium zirconium matt frit
- Fusion Frit F-579
Zinc free calcium frit
- Fusion Frit F-582
Lithium frit
- Fusion Frit F-585
- Fusion Frit F-586 - Alkaline boron frit
- Fusion Frit F-588
Zinc free calcium frit
- Fusion Frit F-592
Alkaline boron frit
- Fusion Frit F-60
Zinc free calcium and sodium frit
- Fusion Frit F-611
Barium frit
- Fusion Frit F-65
High barium boron frit
- Fusion Frit F-69
Low expansion magnesium frit
- Fusion Frit F-71
Alkaline flux for grinding wheels
- Fusion Frit F-74
Alkaline boron flux
- Fusion Frit F-75
Bond Frit
- Fusion Frit F-76
- Fusion Frit F-77
BOND FRIT
- Fusion Frit F-79
Low expansion flux for high alumina bodies
- Fusion Frit F-95
Opacified flux for wall tile
- Fusion Frit F644
High-sodium boron-free frit
- Fusion Frit FL-1
Calcium lead borosilicate frit
- Fusion Frit FL-17
- Fusion Frit FL-28
- Fusion Frit FL-308
- Fusion Frit FL-31
Cadmium frit for cadmium/selenium class colors
- Fusion Frit FL-39
- Fusion Frit FL-4
- Fusion Frit FL-42
- Fusion Frit FL-43
- Fusion Frit FL-46
- Fusion Frit FL-51
- Fusion Frit FL-55
- Fusion Frit FL-99
- Fusion Frit FZ-10
Zircon alkaline boro silicate frit
- Fusion Frit FZ-14
Zinc low boron frit
- Fusion Frit FZ-16
SODA ZINC BOROSILICATE LEADLESS FRIT
- Fusion Frit FZ-164
Zinc calcium alkaline frit
- Fusion Frit FZ-22
Zinc barium calcium frit
- Fusion Frit FZ-23
- Fusion Frit FZ-24
High expansion leadless frit
- Fusion Frit FZ-241
High expansion frit
- Fusion Frit FZ-25
Boro Sodium Frit, Tile Flux
- Fusion Frit FZ-276
- Fusion Frit FZ-284
Zircon frit
- Fusion Frit FZ-30
Zinc barium artware, tile, sanitaryware glaze frit
- Fusion Frit FZ-35
- Fusion Frit FZ-376
- Fusion Frit FZ-376A
Fast fire Opaque Frit
- Fusion Frit FZ-390
Low zinc frit
- Fusion Frit FZ-430
Calcium zinc frit
- Fusion Frit FZ-45
- Fusion Frit FZ-557
Fast fire transparent zinc frit
- Fusion Frit FZ-576
Ca-Zn transparent monoporosa frit
- Fusion Frit FZ-580
Fast fire zinc opaque frit
- Fusion Frit FZ-583
Barium Zinc Zero Boron frit
- Fusion Frit FZ-589
- Fusion Frit FZ-6
- Fusion Frit FZ-647
- Fusion Frit FZ-81
Mystery frit without exact chemistry
- Fusion Frit FZ-84
Zinc alkaline frit
- Fusion Frit FZ-9
- General Frit 400F
- General Frit GF-100
Opacified all-fritted tile glaze frit
- General Frit GF-103
Calcium sodium borosilicate for partially fritted tile glazes
- General Frit GF-104
Zinc bearing frit for use in all-fritted glazes
- General Frit GF-106
High-sodium high expansion frit
- General Frit GF-108
- General Frit GF-109
Sodium calcium borosilicate used in tile glazes
- General Frit GF-110
Zinc sodium frit for textured tile glazes
- General Frit GF-111
SODIUM CALCIUM BOROSILICATE
- General Frit GF-112
All-fritted glaze for semi-vitreous dinnerware
- General Frit GF-113
Leadless High Boron/lime Glaze Frit
- General Frit GF-114
Leadless High Expansion
- General Frit GF-115
High Calcium Boron Leadless for partially-fritted tile glazes
- General Frit GF-118
Frit used for all-fritted semi-opacified tile glazes
- General Frit GF-125
CALCIUM BOROSILICATE
- General Frit GF-126
- General Frit GF-127
ALL-FRITTED GLAZE
- General Frit GF-129
High barium borosilicate leadless frit
- General Frit GF-134
High Alkali Leadless Low Boron
- General Frit GF-136
High Potassium
- General Frit GF-14
CALCIUM LEAD BORON FRIT
- General Frit GF-140
High boron high lithium frit for bonding abrasives
- General Frit GF-141
High potassium high alumina bonding frit for abrasives
- General Frit GF-143
Sodium Boron Silicate Leadless
- General Frit GF-144
Low expansion high magnesia borosilicate frit
- General Frit GF-146
High sodium zinc borate frit (no silica)
- General Frit GF-15
Clear leaded frit for all-fritted cone 06 glazes
- General Frit GF-150
Fast fire frit for partially fritted tile glazes
- General Frit GF-154
HIGH STRONTIUM BOROSILICATE
- General Frit GF-156
LITHIUM BOROSILICATE
- General Frit GF-160
LEADFREE
- General Frit GF-18
Leaded calcium frit for cone 01-5 dinnerware glazes
- General Frit GF-20
Clear leaded glaze for chrome-tin pink all-fritted glazes
- General Frit GF-25
Cadmium frit for make cadmium selenium colors
- General Frit GF-27
Medium lead frit cone 06-04 all-fritted hobby/artware glazes
- General Frit GF-42
High lead very low melting frit
- General Frit GF-509
- General Frit GF-8
LOW EXPANSION
- General Frit GF-9
High Lead Zincless Glaze Frit
- General Frit L-294-J
- Glostex Frit 32
- Glostex Frit H-2
- Heraeus Schauer Frit K 1325
High-sodium low alumina frit
- Heraeus Schauer Frit K 1562
Lead sodium zero alumina frit
- Heraeus Schauer Frit K 3066
Lead sodium zero alumina frit
- Hommel Frit 1005
- Hommel Frit 1006
- Hommel Frit 1007
- Hommel Frit 1020
- Hommel Frit 1021
- Hommel Frit 1030
- Hommel Frit 11
Medium lead zinc frit
- Hommel Frit 13
High Lead Frit
- Hommel Frit 14
Leadless calcium leadless zero alumina borosilicate
- Hommel Frit 154
- Hommel Frit 160
Medium lead calcium borosilicate
- Hommel Frit 166
- Hommel Frit 18
- Hommel Frit 183
- Hommel Frit 2106
Sodium antimony frit
- Hommel Frit 22
Low Lead Frit Boron Frit
- Hommel Frit 220
- Hommel Frit 24
- Hommel Frit 240
High Lead Boron Frit
- Hommel Frit 242
Borosilicate frit
- Hommel Frit 25
Leadless Sodium Boron Frit
- Hommel Frit 259
Leadless, use for cone 06-02
- Hommel Frit 266
Leadless High Calcia Boron Frit
- Hommel Frit 267
Leadless Borosilicate Frit
- Hommel Frit 27
- Hommel Frit 276
- Hommel Frit 28
- Hommel Frit 285
Leadless Alkaline Frit
- Hommel Frit 28F198
- Hommel Frit 290
- Hommel Frit 2GF11C
- Hommel Frit 2GF128B
- Hommel Frit 2GF145C
- Hommel Frit 2GF176D
LEADED
- Hommel Frit 2GF188
- Hommel Frit 2GF241A
- Hommel Frit 2GF27D
- Hommel Frit 2GF37C
- Hommel Frit 2GF56A
- Hommel Frit 2GF56C
- Hommel Frit 2GF64A
- Hommel Frit 2GF65E
- Hommel Frit 2GF6K
- Hommel Frit 316
- Hommel Frit 33
High lead frit
- Hommel Frit 334
- Hommel Frit 344
Low lead calcium borate frit
- Hommel Frit 361
- Hommel Frit 367
- Hommel Frit 373
Leaded glaze frit
- Hommel Frit 378
- Hommel Frit 378A
- Hommel Frit 381
- Hommel Frit 383
- Hommel Frit 385
High barium frit
- Hommel Frit 389
Strontium calcium silicate frit
- Hommel Frit 399
- Hommel Frit 3GF132E
- Hommel Frit 3GF13C
- Hommel Frit 3GF195B
- Hommel Frit 3GF222A
- Hommel Frit 3GF238B
- Hommel Frit 3GF267C
- Hommel Frit 3GF272B
- Hommel Frit 3GF272C
- Hommel Frit 3GF276C
- Hommel Frit 3GF61A
LEADLESS FRIT
- Hommel Frit 3GF84C
- Hommel Frit 400
Leadless barium frit
- Hommel Frit 402
- Hommel Frit 403
- Hommel Frit 419
- Hommel Frit 432
- Hommel Frit 435
- Hommel Frit 437
Lead alumina bilsilicate (small amount of alkali)
- Hommel Frit 440
Sodium borate zirconium frit (1% lead)
- Hommel Frit 441
Low lead calcium zinc borate frit
- Hommel Frit 442
Leadless calcium magnesium borosilicate frit
- Hommel Frit 445
- Hommel Frit 446
Leadless zinc high boron frit
- Hommel Frit 447
Low lead calcium borate frit
- Hommel Frit 448
Leaded low alumina low borax calcium frit
- Hommel Frit 450
Medium lead low alumina borax frit
- Hommel Frit 465
- Hommel Frit 468
- Hommel Frit 472
- Hommel Frit 474
- Hommel Frit 477
- Hommel Frit 482
Barium zinc frit
- Hommel Frit 486
Calcium strontium borosilicate frit
- Hommel Frit 487
- Hommel Frit 488
- Hommel Frit 49
- Hommel Frit 490
- Hommel Frit 493
Leaded calcium borosilicate frit
- Hommel Frit 494
Leadless strontium barium frit
- Hommel Frit 497
Zinc magnesia borosilicate frit
- Hommel Frit 498
- Hommel Frit 4GF113A
- Hommel Frit 4GF135E
- Hommel Frit 4GF137A
- Hommel Frit 4GF137C
- Hommel Frit 4GF148E
- Hommel Frit 4GF151B
- Hommel Frit 4GF152E
- Hommel Frit 4GF153A
- Hommel Frit 4GF154D
- Hommel Frit 4GF156B
- Hommel Frit 4GF164E
- Hommel Frit 4GF171B
- Hommel Frit 4GF173D
- Hommel Frit 4GF175B
- Hommel Frit 4GF40E
- Hommel Frit 4GF45C
- Hommel Frit 4GF48B
- Hommel Frit 4GF52A
- Hommel Frit 4GF53C
- Hommel Frit 4GF56E
- Hommel Frit 4GF57B
- Hommel Frit 4GF63A
- Hommel Frit 4GF63D
- Hommel Frit 4GF65B
- Hommel Frit 4GF71D
- Hommel Frit 4GF79D
- Hommel Frit 4GF93E
- Hommel Frit 4GF95D
- Hommel Frit 5
- Hommel Frit 509
- Hommel Frit 520
- Hommel Frit 529
Leadless high sodium low alumina low boron frit
- Hommel Frit 536
- Hommel Frit 542
- Hommel Frit 550
Leadless calcium borax frit
- Hommel Frit 555
- Hommel Frit 566
- Hommel Frit 571
- Hommel Frit 573
High lead zinc frit
- Hommel Frit 574
- Hommel Frit 576
Calcium borosilicate very low lead frit
- Hommel Frit 579
- Hommel Frit 581
- Hommel Frit 584
Lead monoborate frit
- Hommel Frit 595
Leaded barium calcium strontium silicate frit
- Hommel Frit 61
- Hommel Frit 630
Leadless strontium frit
- Hommel Frit 634
- Hommel Frit 642
Leadless alkali zinc flourine borosilicate frit
- Hommel Frit 64B
- Hommel Frit 69
- Hommel Frit 698
Zircon borosilicate frit
- Hommel Frit 71
- Hommel Frit 71
LEADED FRIT
- Hommel Frit 840
- Hommel Frit 90
Leadless Frit
- Hommel Frit G-26
Zinc barium artware, sanitaryware and tile glaze frit
- Hommel Frit K-3
Leadless Frit
- Hommel Frit RW238E
- Hommel Frit T-206
- Hommel Frit T-88
- James Kent Frit 2917X0
OPAQUE (FORMERLY #90401018)
- James Kent Frit D9991
Low zinc borax frit (formerly #90400045)
- James Kent Frit DR1327
Zinc barium calcium alkali frit (formerly #FT0540)
- James Kent Frit DR1328
TRANSPARENT (FORMERLY #FT0541)
- James Kent Frit F12
Opaque (formerly #90401026)
- James Kent Frit N4129
TRANSPARENT (FORMERLY #90400023)
- James Kent Frit SN121
OPAQUE (FORMERLY #90401050)
- James Kent Frit SN70
OPAQUE (FORMERLY #90401034)
- James Kent Frit SN72
TRANSPARENT (FORMERLY #FTO517)
- James Kent Frit SN97
OPAQUE (FORMERLY #90401030)
- Johnson Matthey Frit 169
Barium frit
- Johnson Matthey Frit 623
B33X7, MOK623
- Matrix Frit B40-C
High boron zero silicate refractory calcia alumina frit
- Matrix Frit B70-A
High boron zero silicate calcia alumina frit
- Matthey Frit 20126
- Matthey Frit 20306G
Calcium boro silicate frit
- Matthey Frit 21065g
GLAZE LEAD BORAX
- Matthey Frit 3701F
General purpose alkaline frit
- Mondre and Manz Frit 1233
- Mondre and Manz Frit 4067
Barium zinc potash low alumina leaded frit
- Pemco Frit 3185
- Pemco Frit 3191
- Pemco Frit 3211
- Pemco Frit 3V128
- Pemco Frit J-22
- Pemco Frit J-224
- Pemco Frit J-239
- Pemco Frit J-241
- Pemco Frit J-344
- Pemco Frit J-394
- Pemco Frit J-43
- Pemco Frit P-1000
LEADLESS FRIT
- Pemco Frit P-1084
- Pemco Frit P-1090
Leadless borax frit for semi matte glazes
- Pemco Frit P-1154
- Pemco Frit P-1225
- Pemco Frit P-1409
Low expansion high magnesia alkali-free leadless glaze frit
- Pemco Frit P-1413
Calcium-borosilicate flux
- Pemco Frit P-1492
- Pemco Frit P-1679
- Pemco Frit P-1701
LEADLESS FRIT
- Pemco Frit P-1733
Soda-zinc-borosilicate leadless frit
- Pemco Frit P-1734
- Pemco Frit P-1836
Leadless, high zinc, all-fritted glaze
- Pemco Frit P-1853
- Pemco Frit P-1855
Very low expansion borosilicate glass
- Pemco Frit P-1941
- Pemco Frit P-1A43
Low expansion high zinc borosilicate
- Pemco Frit P-1A44
Low expansion high zinc high boron frit
- Pemco Frit P-1F07
High CaO/Na2O/ZnO borosilicate low alumina frit
- Pemco Frit P-1J81
Semi-opaque all-fritted glaze for cone 02-4
- Pemco Frit P-1N72
Alkali-alumina-borosilicate body frit
- Pemco Frit P-1R41
Leadless flux for Cone 06
- Pemco Frit P-1R63
- Pemco Frit P-1T27
High expansion zirconia fluorine frit
- Pemco Frit P-1V04
High sodium low boron low alumina body and glaze flux
- Pemco Frit P-1V31
Semi-opaque high zinc fast fire frit
- Pemco Frit P-1X24
- Pemco Frit P-2201
Calcium borate frit, Gerstley Borate substitute
- Pemco Frit P-238
LEADLESS FRIT
- Pemco Frit P-239
- Pemco Frit P-25
Leadless alkaline fluorine frit, use for cone 06-02
- Pemco Frit P-278
- Pemco Frit P-283
High expansion boron free frit
- Pemco Frit P-2C05
Alkaline body flux
- Pemco Frit P-2C59
Semi-opaque fast fire frit
- Pemco Frit P-2D27
Leadless frit for use at cone 02-10
- Pemco Frit P-2D50
Semi-opaque 1900-2000F fast fire for all-fritted glazes
- Pemco Frit P-2D71
Leadless alkaline fluorine frit
- Pemco Frit P-2G63
Highly opaque frit for use in all-fritted cone 06-6 glazes
- Pemco Frit P-2J57
High expansion low melting phosphate based glass
- Pemco Frit P-2N87
High alkali, low alumina, low boron leadless frit
- Pemco Frit P-2P36
Lithium-based ultra-low expansion frit for all-fritted glazes
- Pemco Frit P-2V25
Low temperature flux frit used in brick coatings
- Pemco Frit P-311
Calcium borosilicate frit for partially fritted dinnerware glazes
- Pemco Frit P-318
Leadless high barium zero alumina borosilicate flux
- Pemco Frit P-349
- Pemco Frit P-3E12
Semi-opaque all-fritted glaze for cone 02-4
- Pemco Frit P-3K51
- Pemco Frit P-3T355
- Pemco Frit P-3T928
- Pemco Frit P-3V126
Opaque tile frit
- Pemco Frit P-404
High temperature leadless boron free glaze flux
- Pemco Frit P-4D79
- Pemco Frit P-4K05
- Pemco Frit P-4K47
Strontium sanitaryware frit
- Pemco Frit P-4N57
- Pemco Frit P-54
Sodium-calcium-borosilicate low melting flux
- Pemco Frit P-586
Barium, zinc, calcium frit for partially fritted cone 4-10 glazes
- Pemco Frit P-609
LEADLESS FRIT
- Pemco Frit P-626
Low fire high-barium leadless borosilicate
- Pemco Frit P-64
Low temperature leadless all-fritted 08-02 glaze
- Pemco Frit P-658
Leaded strontium low boron high alumina frit
- Pemco Frit P-67
Sodium-potassium-alumina-borosilicate flux
- Pemco Frit P-688
LEADLESS FRIT
- Pemco Frit P-757
Opaque crackle glaze component for cone 06
- Pemco Frit P-760
Cadmium bearing frit
- Pemco Frit P-786
Leadless all-fritted glaze
- Pemco Frit P-802
Leadless flux for cone 06 glazes
- Pemco Frit P-827
Leadless boron free frit for high temperature
- Pemco Frit P-83
Medium Lead Frit
- Pemco Frit P-830
Leadless Frit
- Pemco Frit P-835
Not fluorine version of frit P-2D27
- Pemco Frit P-878
Zirconium opacified frit
- Pemco Frit P-926
Leadless fast fire frit
- Pemco Frit P-930
Leadless all-fritted base
- Pemco Frit P-941
Magnesia-alumina-silica eutectic
- Pemco Frit P-991
All-fritted base for high talc bodies cone 02-2
- Pemco Frit Pb-1038
All-fritted base for chome-alumina pink stains
- Pemco Frit Pb-1041
LEADED FRIT
- Pemco Frit Pb-106
Lead high calcium frit for dinnerware glazes
- Pemco Frit Pb-1114
Calcium borosilite medium lead frit for cone 08-04 glazes
- Pemco Frit Pb-113
Very low melting high lead frit
- Pemco Frit Pb-1151
Leaded titanium frit
- Pemco Frit Pb-1241
Leaded sodium and potassiun free frit
- Pemco Frit Pb-1279
Very low lead barium frit for partially fritted glazes cone 04-5
- Pemco Frit Pb-1307
High lead zinc containing wall tile frit
- Pemco Frit Pb-1325
High lead borosilicate with small amount of sodium
- Pemco Frit Pb-1421
Leaded low borax frit
- Pemco Frit Pb-1492
LEADED FRIT
- Pemco Frit Pb-1931
- Pemco Frit Pb-1951
Lead-borosilicate flux
- Pemco Frit Pb-197
Zinc bearing lead frit for all-fritted glaze cone 04-6
- Pemco Frit Pb-1B20
Lead-alumina-silicate low expansion frit
- Pemco Frit Pb-1K-75
- Pemco Frit Pb-1K75
Cone 06 all-fritted transparent gloss glaze
- Pemco Frit Pb-1M90
Titanium bearing matte glaze component at Cone 01
- Pemco Frit Pb-1N84
Very low melting high lead borosilicate
- Pemco Frit Pb-1N86
Cone 1 glaze with 50% clay addition
- Pemco Frit Pb-1R-43
- Pemco Frit Pb-1R40
Used in Cone 06 matte glazes
- Pemco Frit Pb-1R99
High expansion lead flux for cone 06 glazes
- Pemco Frit PB-1V48
Leaded cadmium frit for orage/red colors cone 08-06
- Pemco Frit Pb-1X22
- Pemco Frit Pb-2C52
All-fritted opaque leaded glaze
- Pemco Frit Pb-2F-35
- Pemco Frit Pb-2F35
All-fritted dinnerware glaze at Cone 1 to 4
- Pemco Frit Pb-2G12
Cadmium frit
- Pemco Frit Pb-2G30
Low lead calcium frit
- Pemco Frit Pb-2V93
Boron-free, zinc bearing leaded dinnerware glaze cone 4
- Pemco Frit Pb-316
Lead-alumina-sillicate eutectic
- Pemco Frit Pb-349
Lead bearing, zincless, all-fritted glaze
- Pemco Frit Pb-40
- Pemco Frit Pb-41
Zinc-lead-borosilicate very low melting flux cone 08-8
- Pemco Frit Pb-461
Very low expansion lead-borosilicate
- Pemco Frit Pb-545
Lead bisilicate
- Pemco Frit Pb-589
Zirconium opacified version of Pb-197
- Pemco Frit Pb-63
Medium lead frit
- Pemco Frit Pb-674
Low expansion (low alkalia) low-lead glaze frit
- Pemco Frit Pb-700
Lead alumina bilsilicate frit (1% alumina)
- Pemco Frit Pb-704
Zinc bearing, all-fritted base for cone 1-6
- Pemco Frit Pb-71
- Pemco Frit Pb-716
Calcium-lead-silicate frit
- Pemco Frit Pb-723
Soda-lead-alumina-silicate low melting glaze frit
- Pemco Frit Pb-740
High zinc frit for matte glazes cone 06-4
- Pemco Frit Pb-742
Leaded zincless frit cone 08-1.
- Pemco Frit Pb-801
Lead-bearing flux for cone 06
- Pemco Frit Pb-83
Soda-high lead-borosilicate very low melting frit
- Pemco Frit Pb-906
All-fritted opaque glaze
- Pemco Frit Pb-943
Low lead flux for cone 06 glazes
- Pemco Frit Pb-967
- Potclays Frit 2261
Lead alumina bilsilicate frit
- Potclays Frit 2262
Lead Frit
- Potclays Frit 2263
High calcium borosilicate frit
- Potclays Frit 2265
- Potclays Frit 2266
This is actually Ferro Frit 3110
- Potclays Frit 2268
Very high calcium borosilicate frit
- Potclays Frit 2269
This is actually Ferro Frit 3195
- Potclays Frit 2270
White Zircon Frit
- Potclays Frit 2272
This is actually Ferro Frit 3124
- Potclays Frit 2273
This is actually Ferro Frit 3134
- Potclays Frit 2275
Very high alkali frit
- Potclays Frit 2279
Alkali free calcium lithium magnesia zinc borosilicate frit
- Potclays Frit 2281
Lead alumina bisilicate frit
- Roudnice Frit 02291
Czech Frit
- Solargil Frit FR1
Monosilicate lead frit
- Solargil Frit FR10
Calcium borate low alumina frit
- Solargil Frit FR2
Lead bisilicate frit
- Solargil Frit FR3
Calcium borate frit
- Solargil Frit FR4
Low alumina frit
- Solargil Frit FR5
Zinc zero alumina frit
- Solargil Frit FR6
Lead barium boron frit
- Solargil Frit FR7
Alkaline frit
- Solargil Frit FR8
Calcium borate frit
- Solargil Frit FR9
Zircon frit
Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
|
|
INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()
|