Digitalfire Ceramic Materials Database

Logged in as Level 2 access: Logout


Boraq 3

Plainsman Plastic Gerstley Borate Substitute

Chemistry %

CaO27.30
MgO2.00
K2O0.50
Na2O3.20
Al2O32.40
B2O326.50
SiO211.90
Fe2O30.10
 

Volatiles %

LOI26.05

Boraq 3 is derived from Boraq 2 to provide an alternative in cases where the presense of CaO is preferable to MgO.


Out Bound Links

In Bound Links

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?>
<material name="Boraq 3" descrip="Plainsman Plastic Gerstley Borate Substitute" searchkey="" loi="0.00" casnumber="167077-83-0">
<oxides>
<oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="27.300" tolerance=""/>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="U" percent="2.000" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="U" percent="0.500" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="3.200" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.400" tolerance=""/>
<oxide symbol="B2O3" name="Boric Oxide" status="U" percent="26.500" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="11.900" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="LOI" name="Loss on Ignition" percent="26.050" tolerance=""/>
</volatiles>
</material>



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()