Alkatrol G-20041

Chemistry %

K2O1.25
Na2O1.25
TiO20.40
Al2O315.00
SiO277.30
Fe2O32.20
 

Volatiles %

LOI2.60

Out Bound Links

In Bound Links

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?>
<material name="Alkatrol G-20041" descrip="" searchkey="" loi="2.60" casnumber="12269-78-2">
<oxides>
<oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.250" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.250" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.400" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="15.000" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="77.300" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.200" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="LOI" name="Loss on Ignition" percent="2.600" tolerance=""/>
</volatiles>
</material>



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()