Digitalfire Library Reference Database

Logged in as Level 2 access: Logout


Library: Evaluating Particle Size by Scott Baker and Tim Herrman


A comprehensive discussion of particle physical size analysis using sieves and related equipment. An array of computational analyses are also covered. Paper is from Kansas State University Agricultural Experiment Station.